How to apply:
- Use thin rubber protective gloves.
- Apply indoor only with temperature of 18-24 C.
- Shake bottle well before using.
- Make sure the surface is dry, clean and cool.
- Spread evenly with applicator on one part of the paint.
- Buff with microfiber cloth to a high gloss. Don’t wait too long with buffing after spreading the product.
- Move to next paintwork section.
- Drying time after application – 4 hours.
Note:
- It is best to use SLS as on top finish for permanent ceramic coating as Q7, Q10, or T1.
- Remember to degrease the surface if SLS is applied as the only coating.